- 产品详情
-
产品品牌阿科玛
产品产地法国
-
产品型号kynar 740
包装规格25kg
Kynar® 740 resin
Kynar® resins are fluorinated thermoplastic homopolymers.
Outstanding characteristics: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermo-mechanical properties.
Main applications: corrosion protection in the chemical industry, coating (painting, co-extrusion), off-shore, wire and cable.
Kynar® 740 resin is a standard grade of granules for extrusion of tubes and plaques, compression and transfer molding. This product is ANSI/NSF Standard 61 certified.
A powder form is available as Kynar® 741 resin.
Kynar® resins are fluorinated thermoplastic homopolymers.
Outstanding characteristics: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermo-mechanical properties.
Main applications: corrosion protection in the chemical industry, coating (painting, co-extrusion), off-shore, wire and cable.
Kynar® 740 resin is a standard grade of granules for extrusion of tubes and plaques, compression and transfer molding. This product is ANSI/NSF Standard 61 certified.
A powder form is available as Kynar® 741 resin.
流变性能 | 价值 | 单位 | 测试标准 |
熔体体积流动速度, MVR | 1.1 | cm³/10min | ISO 1133 |
温度 | 230 | °C | - |
载荷 | 5 | kg | - |
模塑收缩率, 平行 | 2.0 | % | ISO 294-4, 2577 |
模塑收缩率, 垂直 | 2.0 | % | ISO 294-4, 2577 |
机械性能 | 价值 | 单位 | 测试标准 |
拉伸模量 | 1700 | MPa | ISO 527-1/-2 |
屈服应力 | 50 | MPa | ISO 527-1/-2 |
屈服伸长率 | 7 | % | ISO 527-1/-2 |
名义断裂伸长率 | >50 | % | ISO 527-1/-2 |
拉伸蠕变模量, 1h | 1050 | MPa | ISO 899-1 |
拉伸蠕变模量, 1000h | 570 | MPa | ISO 899-1 |
无缺口简支梁冲击强度, +23°C | 244 | kJ/m² | ISO 179/1eU |
简支梁冲击强度, -30°C | 186 | kJ/m² | ISO 179/1eU |
简支梁缺口冲击强度, +23°C | 14 | kJ/m² | ISO 179/1eA |
简支梁缺口冲击强度, -30°C | 5 | kJ/m² | ISO 179/1eA |
热性能 | 价值 | 单位 | 测试标准 |
熔融温度, 10°C/min | 168 | °C | ISO 11357-1/-3 |
玻璃化转变温度, 10°C/min | -40 | °C | ISO 11357-1/-2 |
热变形温度, 1.80 MPa | 105 | °C | ISO 75-1/-2 |
热变形温度, 0.45 MPa | 135 | °C | ISO 75-1/-2 |
维卡软化温度, 50°C/h 50N | 135 | °C | ISO 306 |
线性热膨胀系数, 平行 | 150 | E-6/K | ISO 11359-1/-2 |
1.5mm名义厚度时的燃烧性 | V-0 | class | IEC 60695-11-10 |
测试用试样的厚度 | 1.6 | mm | - |
Yellow Card 现存 | 是的 | - | - |
厚度为h时的燃烧性 | V-0 | class | IEC 60695-11-10 |
测试用试样的厚度 | 0.8 | mm | - |
燃烧性-氧指数 | 43 | % | ISO 4589-1/-2 |
电性能 | 价值 | 单位 | 测试标准 |
相对介电常数., 100Hz | 11 | - | IEC 60250 |
相对介电常数., 1MHz | 8 | - | IEC 60250 |
介质损耗因子, 100Hz | 260 | E-4 | IEC 60250 |
介质损耗因子, 1MHz | 2310 | E-4 | IEC 60250 |
体积电阻率 | 2E12 | Ohm*m | IEC 60093 |
表面电阻率 | >1E15 | Ohm | IEC 60093 |
介电强度 | 21 | kV/mm | IEC 60243-1 |
相对漏电起痕指数 | 600 | - | IEC 60112 |
其它性能 | 价值 | 单位 | 测试标准 |
吸水性 | 0.03 | % | 类似ISO 62 |
吸湿性 | 0.015 | % | 类似ISO 62 |
密度 | 1780 | kg/m³ | ISO 1183 |
试样制备条件 | 价值 | 单位 | 测试标准 |
注塑, 熔体温度 | 230 | °C | ISO 294 |
注塑, 模具温度 | 90 | °C | ISO 10724 |
注塑, 注射速度 | 10 | mm/s | ISO 294 |
注塑, 保压压力 | 13 | MPa | ISO 294 |
压缩, 模具温度 | 225 | °C | ISO 293 |
压缩, 保压时间 | 3 | min | ISO 293 |
压缩, 脱模温度 | 120 | °C | ISO 293 |
函数
特征
加工方法
异型材挤出成型, 片材挤出成型, 其它挤出成型, 模压/烧结成型, 热成型
供货形式
粒料
特殊性能
经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的
【版权声明】秉承互联网开放、包容的精神,凯茵化工欢迎各方(自)媒体、机构转载、引用我们原创内容,但要严格注明来源凯茵化工;同时,我们倡导尊重与保护知识产权,如发现本站文章存在版权问题,烦请将版权疑问、授权证明、版权证明、联系方式等,发邮件至 app@shkingchem.com,我们将第一时间核实、处理。